https://doi.org/10.15407/iopt.2023.58.136
Optoelectron. Semicond. Tech. 58, 136-146 (2023)
O.M. Kamuz, D.M. Khmil, P.O. Tytarenko, V.S. Kretulis, I.E. Minakova, B.A. Snopok
THE METHODOLOGY FOR DETERMINING LIGHT ABSORPTION COEFFICIENTS OF LUMINOPHORE POWDER YAG:CE3+ MICROPARTICLES AND ITS TECHNOLOGICAL SUPPORT
The development of methods for photometric control of turbid media based on YAG:Ce3+ phosphor (luminophore) microcrystals in transparent matrices requires solving a number of technological problems in the manufacture of self-supporting films of the composite material, adequate measurement of their optical properties and calculation of the corresponding values of absorption indices. This general problem is solved in this work by developing original measuring equipment, elaborating a number of technological protocols and a calculation algorithm based on modelling in the concept of a composite film of a dispersion medium. It is proved that the production of a suspension of microparticles of YAG:Ce3+ powder in epoxy resin at reduced pressure using an original turbine microstirrer allows to obtain a homogeneous and degassed suspension with a low rate of solid particle deposition, efficient light absorption of excitation radiation and an increased level of quantum yield of luminescence. A methodology for manufacturing self-supporting films from the obtained suspension has been developed. Such films are characterised by a low scatter of colourimetric parameters on the surface due to their high spatial homogeneity. 5 ml of the suspension is enough to produce a set of 30 flat-parallel films with an area of up to 1 cm2 and a thickness of 110÷600 µm with an error not exceeding ±3 µm. On the basis of the matrix spectroradiometer НAAS-2000, a photometric measuring setup was developed and created, which, in addition to the spectroradiometer, includes an optical module and an LED blue light source with λmax= 456 nm to excite the luminescence of the light-converting composition layers. The elements of the optical module ensure that the solid angle of the source radiation corresponds to the numerical aperture of the receiver (Ω = 0.126 steradian) in the form of the end window of the fibre-optic cable of the spectroradiometer and cause the transmission of the image on a 1:1 scale. An algorithm for determining the volumetric and linear absorption coefficients of a microcrystal-averaged YAG:Ce3+ phosphor powder under conditions corresponding to the isotropic scattering mechanism was proposed and worked out. Calculations in the composite film model, which takes into account the effects of light absorption and reflection by individual microcrystals in the volume of a transparent matrix, using the results of experimental measurements, allowed us to establish the values of the volume and linear absorption coefficients of the size-averaged (5.3 μm) YAG:Ce3+ microcrystal, which are 774 cm-1 and 129 cm-1, respectively.
Keywords: light absorption coefficient, yttrium-aluminum garnet, luminophore, white LED.
References
1. Khmil D.N., Kamuz A.M., Oleksenko P.F., Kamuz V.G., Aleksenko N.G., Kamuz O.A. Lyuminofory v belykh svetodiodakh: preimushchestva i nedostatki (obzor). Optoelektronika i poluprovodnikovaya tekhnika. 2012. Vyp. 47. S.5-23
2. Khmil D.N., Kamuz A.M., Oleksenko P.F., Kamuz V.G., Aleksenko N.G., Kamuz O.A. Method for determination of the absorption coefficient in films based on photoluminophore suspension for white LEDs. Semiconductor Physics, Quantum Electronics & Optoelectronics. 2015. 18, №2. P. 215-219.
3. Khmil D.N., Kamuz A.M., Oleksenko P.F., Kamuz V.G., Aleksenko N.G., Kamuz O.A. Determination of the spectral dependence for the absorption coefficient of phosphor inorganic microparticles. Semiconductor Physics, Quantum Electronics & Optoelectronics. 2015. 18, № 3. P. 334-340.
4. Strenk F. Peremeshivaniye i apparaty s meshalkami. Per. s. polsk. pod. red. Shchuplyaka I.A. Moskva: Khimiya. 1975. 384 s.
5. Kholand F., Chapman F. Khimicheskiye reaktory i smesiteli dlya zhidkikh protsessov. Moskva: Khimiya. 1974. 208 s.
6. Lianming Wang, Liqiang Zhuang, Hao Xin, Yuexia Huang, Deqiang Wang. Semi-Quantitative Estimation of Ce3+/Ce4+ Ratio in YAG:Ce3+ Phosphor under Different Sintering Atmosphere. Open Journal of Inorganic Chemistry. 2015. 5, №1. P.12-18.
7. Nishankovsky S.V., Dan’ko A.Ya., Puzikov V.M., Savvin Yu.N., Trushkovsky A.G., Krivonogov S.I. Optical and luminescence characteristics of YAG:Ce crystals grown by horizontal directed crystallization in reducing gas medium. Functional materials. 2008. 15, №4. P.546-549.
О.М. Камуз, Д.М. Хміль, П.О. Титаренко, В.С. Кретуліс, І.Є. Мінакова, Б.А. Снопок
Методика визначення показникА поглинання світла мікрочастинками ПОРОШКУ Люмінофора YAG:Сe3+ та її технологічне забезпечення
Розроблення методів фотометричного контролю мутних середовищ на основі мікрокристалів люмінофора YAG:Се3+ в прозорих матрицях потребує вирішення низки технологічних проблем при виготовленні самонесучих плівок композиційного матеріалу, адекватного вимірювання їхніх оптичних властивостей та розрахунку відповідних величин показників поглинання. Ця загальна задача в даній роботі вирішена шляхом розробки оригінального вимірювального устаткування, опрацювання низки технологічних протоколів та алгоритму розрахунку на основі моделювання в концепції композитної плівки дисперсійного середовища. Доведено, що виготовлення суспензії мікрочастинок порошку YAG:Се3+ в епоксидній смолі при зниженому тиску з використанням оригінального турбінного мікроперемішувача дозволяє отримати гомогенну та дегазовану суспензію з низькою швидкістю осаджування твердих частинок, ефективним світлопоглинанням збуджуючого випромінювання і підвищеним рівнем квантового виходу люмінесценції. Розроблено методику виготовлення із отриманої суспензії самонесучих плівок, які відрізняються низьким розкидом значень колориметричних параметрів по поверхні, що обумовлено їхньою високою просторовою однорідністю. 5 мл суспензії достатньо для виготовлення набору з 30 пласкопаралельних плівок площею до 1 см2 і завтовшки 110÷600 мкм з похибкою, що не перевищує ±3 мкм. На базі матричного спектрорадіометра НААS-2000 розроблена і створена вимірювальна фотометрична установка, що містить, крім спектрорадіометра, оптичний модуль і світлодіодне джерело синього випромінювання з λmax= 456 нм для збудження люмінесценції шарів світлоконвертуючої композиції. Елементи оптичного модуля забезпечують відповідність тілесного кута випромінювання джерела до чисельної апертури приймача (Ω=0,126 стерадіан) у вигляді торцевого вікна волоконно-оптичного кабелю спектрорадіометра і обумовлюють передачу зображення в масштабі 1:1. Запропоновано та відпрацьовано алгоритм визначення об'ємного та лінійного показників поглинання усередненого за розміром мікрокристала порошку YAG:Се3+ - люмінофору в умовах, що відповідають ізотропному механізму розсіяння. Розрахунки в моделі композитної плівки, яка враховує ефекти поглинання та відбиття світла окремими мікрокристалами в об’ємі прозорої матриці, з використанням результатів експериментальних вимірювань, дозволили встановити значення об'ємного та лінійного показників поглинання усередненого за розміром (5,3 мкм) мікрокристала YAG:Се3+, які складають 774 см-1 та 129 см-1 відповідно.
Ключові слова: показник поглинання світла, ітрій-алюмінієвий гранат, люмінофор, білий світлодіод.